Solid, high-quality pellets are an important precondition for reliable and meaningful XRF analysis. With the PP 40, RETSCH offers a pellet press which produces strong pellets with a smooth surface. The PP 40 features individual pressure force regulation in the range of 0 to 40 t. It combines the advantage of a small benchtop unit with high press forces, which are built up automatically in three steps, ensuring that even difficult materials are pressed perfectly.
Applying, for example, forces of 10 tons, 20 tons, and 30 tons in sequential steps, each with a 20-second hold time, proves advantageous for pellet stability as particles have sufficient time to settle. Pressing the pellets in aluminum cups further augments their stability. Should these measures prove inadequate, incorporating a binder, such as Licowax, offers an effective stabilization method for challenging samples, including metal powders. Typically, a mixture of 10-15 g of the sample with 2 g of Licowax, pressed in three stages as outlined above, yields optimum results. For the mixing process, the Mixer Mill MM 400, equipped with an adapter for holding 8 conical centrifuge tubes, is highly effective. It ensures that samples are mixed uniformly, automatically, and reproducibly.
Wood 4g
Particle size 0.25 mm
Pressing tool 32 mm
20 s each at 10/20/30 tons
Cellulose 7 g
Particle size 0.15 mm
Pressing tool 40 mm
Aluminum cups 40 mm
30 s each at 10/20/30 tons
Slag 40 g
Particle size 0.25 mm
Pressing tool 40 mm
20 s 20 tons
FeSiMg-Granulate 12 g plus 2 g licowax
Particle size 0.10 mm
Pressing tool 40 mm
Aluminum cups
60 s 15/25/35 tons
Due to its ability to produce homogeneous, stable, and accurate samples efficiently and cost-effectively, pellet pressing is a widely adopted method for preparing samples for XRF analysis.
Aplicabilitate | prepararea peleților pentru analize spectrale |
Domenii in care se utilizeaza | chimie/plastic, geologie/metalurgie, materiale de construcții, mediu/reciclare, sticlă/ceramică |
Presiune max. | 40 t, presiune automată |
Forța de presiune | 0 - 40 t (1 - 400 kN) |
Creșterea forței presiunii / timpului de menținere / descreștere: | fix ramp / 1 - 99 s / fix ramp |
Combinații parametru | 10 |
Steel rings (external Ø / internal Ø) | 40 mm / 32 mm (max. pressure force 15 t) 40 mm / 35 mm (max. pressure force 15 t) 51.5 mm / 35 mm (max. pressure force 30 t) |
Aluminium cup (external Ø) | 32 mm (max. pressure force 25 t) / 40 mm (max. pressure force 40 t) |
Alimentare electrica | 100-120 V, 50/60 Hz; 220-240 V, 50/60Hz |
Conectare sursă de alimentare | monofazic |
W x H x D | 335 x 495 x 570 mm |
Masa netă: | 120 kg |
Standard | CE |
Un inel de oțel sau o cupă de aluminiu este poziționată și umplută cu probă în matrița presei PP 40. Întregul ansamblu se introduce apoi sub placa de presare și se inițiază procesul de presare.
Densitatea pulberii crește odata cu creșterea presiunii. Pentru a permite dezvoltarea forțelor de adeziune intre particule, forța maximă de presare trebuie menținută pe un anumit interval de timp. Acest lucru si presarea în trei etape, prin creșterea treptată a presiunii asigură stabilitatea maximă a pastilei obținute.